Just wanted to update
Been running my ported x02 manifold for atleast a week so far
Hanging a PTE SCM5031e off of it (50 trim)
Been boosting around 20 psi, and have done multiple pulls for tuning
Manifold has turned a blueish/light purple color overall. Absolutely NO brown spots, I believe that wiping the manifold down thorougly before heating it, and not touching it when hot or anything has kept it this way. Not to mention, the different grade of a stainless most likely helped.
Been running my ported x02 manifold for atleast a week so far
Hanging a PTE SCM5031e off of it (50 trim)
Been boosting around 20 psi, and have done multiple pulls for tuning
Manifold has turned a blueish/light purple color overall. Absolutely NO brown spots, I believe that wiping the manifold down thorougly before heating it, and not touching it when hot or anything has kept it this way. Not to mention, the different grade of a stainless most likely helped.